What's included
- Pressure wash and clean
- Crack filling if needed
- Two coats of penetrating or topical sealer
- 24-hour cure before traffic
Specifications
| Frequency | Every 3–5 years for exposed aggregate |
|---|---|
| Sealer types | Penetrating (natural look) or topical (wet look) |
| Drying | 24 hours before foot traffic, 72 hours before vehicles |
| Best time | Autumn or spring — avoid extreme heat |
| Best for | Any concrete surface that hasn't been sealed in 3+ years |
| Typical duration | Half a day to 1 day (including dry time) |
How much does concrete sealing cost in Adelaide?
Concrete sealing in Adelaide costs $12–$28/m² for exposed aggregate, and a 60 m² driveway costs $600–$1,600 including cleaning and preparation.
| Surface or extra | Published SA price |
|---|---|
| Exposed aggregate | $12–$28/m² |
| Plain concrete | $8–$20/m² |
| Coloured or stencilled concrete | $15–$30/m² |
| Stripping a failed sealer | $15–$40/m² |
| Anti-slip additive | $2–$6/m² |
| Typical 60 m² driveway | $600–$1,600 |
Penetrating vs topical sealer: which should you choose?
Choose a penetrating sealer for a natural look, long life and grip; choose a topical sealer for a wet look that deepens the stone colour. Topical sealers need redoing more often in Adelaide sun.
| Penetrating (silane-siloxane) | Topical (acrylic) | |
|---|---|---|
| Look | No change, matte | Wet look or satin |
| Lasts | 5–10 years | 2–4 years |
| Can peel or go milky | No | Yes, if moisture is trapped |
| Grip | Unchanged | Reduced unless anti-slip is added |
| Suits | Driveways, paths, pool surrounds | Exposed aggregate and coloured concrete for show |
How often should concrete be resealed in Adelaide?
Reseal exposed aggregate every 3–5 years in Adelaide. North and west-facing driveways in full sun sit at the short end, and a topical sealer there can need redoing after 2–3 years.
The water test tells you when. Sprinkle water on a dry driveway: if it soaks in and darkens the surface instead of beading, the sealer has worn off.
- Full sun, topical sealer: 2–3 years.
- Shaded, topical sealer: 3–4 years.
- Penetrating sealer: 5–10 years.
- Coastal suburbs: salt air shortens the interval to about 2–3 years.
What happens on the day, and when can you use the driveway?
Sealing takes Half a day to 1 day, but cleaning should happen first on a separate day. Sealing over a damp slab is a common cause of white, cloudy patches.
- Clean: pressure wash, degrease oil spots and treat rust or leaf stains.
- Dry: allow several dry days between cleaning and sealing.
- Repair: fill cracks before the sealer goes on.
- Seal: two thin coats. One product data sheet sets a minimum 2 hours between coats.
- Wait: about 24 hours before walking on it. Vehicle access is typically 24–72 hours, and up to 5 days for some solvent sealers.
When is the best time to seal, and can you do it yourself?
Autumn and spring are the best times to seal concrete in Adelaide. Summer heat makes solvent flash off before the sealer levels, which leaves bubbles and lap marks. One manufacturer's data sheet says not to apply sealer below 8°C or above 35°C.
Sealing a sound, clean driveway is a realistic DIY job. Stripping a failed or peeling sealer is not: it involves solvents and costs $15–$40/m² when done by a contractor. Concrete that was never sealed should cure first, usually quoted as 28 days.
Compare other finishes
Common questions
How much does it cost to reseal an exposed aggregate driveway in Adelaide?
Resealing an exposed aggregate driveway in Adelaide costs $12–$28/m². A typical 60 m² driveway costs $600–$1,600 including pressure cleaning and preparation. Stripping an old failed sealer first adds $15–$40/m².
How often should exposed aggregate be resealed?
Every 3–5 years in Adelaide, and every 2–3 years in coastal suburbs or where a topical sealer faces full northern or western sun. Penetrating sealers last longer, at 5–10 years. Use the water bead test to check.
Why has my driveway sealer gone white or milky?
White or milky sealer is usually moisture trapped under a topical coating, often from sealing a damp slab. Mild cases can sometimes be re-dissolved with solvent. Bad cases need stripping at $15–$40/m² and resealing on a dry surface.
Does sealing make concrete slippery?
A gloss topical sealer can. Published SA data shows a high-gloss sealer can drop a P4–P5 exposed aggregate surface to P1–P2. A penetrating sealer leaves grip unchanged, and an anti-slip additive costs $2–$6/m².
Can I seal my driveway myself?
Yes, if the surface is sound and clean. Pressure wash, let the slab dry for several days, then roll on two thin coats in mild weather between 8°C and 35°C. Leave stripping of old peeling sealer to a contractor.
How long after sealing can I drive on the driveway?
Typically 24–72 hours, depending on the product and the weather. Some solvent-based exposed aggregate sealers ask for at least 5 days before vehicles. Foot traffic is usually fine after about 24 hours.
Do I need to seal new exposed aggregate?
Yes. New exposed aggregate is sealed as part of the installation, usually within a day of exposing the stone. Decorative, coloured and exposed aggregate concrete should stay sealed to keep its appearance; plain grey concrete is optional.
How much does concrete sealing & resealing cost in Adelaide?
$12–$28 per m² installed. The final price depends on soil conditions, access, area size and any extras like old surface removal.
Sources
- The Quote Yard: Concrete Sealing SA (sealer types and prices)
- Dulux Avista: Exposed aggregate concrete sealer data sheet
- The Quote Yard: Concrete Pool Surrounds SA (slip ratings by finish)
- What's the Damage: Concreting Cost in Adelaide (prices verified November 2026)
Last reviewed .